Zero-VOC Intumescent Finish Launches

MONDAY, AUGUST 17, 2015


A new zero-VOC intumescent product for wood structures is now available.

PyroTech has created the two-component, thin-film intumescent coating that can be used on existing and new wood structures.

PyroCide Clear is made to produce a clear to light amber, hard, high-gloss finish that will not bubble, crack or haze, the company says.

Wood
PyroTech
PyroCide Clear provides a high-gloss finish that will not bubble or crack, PyroTech has said.
Wood
PyroTech

PyroCide Clear provides a high-gloss finish that will not bubble or crack, PyroTech has said.

The product provides resistance from humidity and water spotting as well as UV rays, according to product literature.

Product Uses

PyroCide Clear can be applied with a brush or spray and does not require a topcoat. However, a topcoat should be used in areas that could be handled or touched frequently, or for those areas that are subject to high humidity, the company says.

NLB Corporation
APV Engineered Coatings

PyroCide Clear offers a Class A flame and smoke rating. It has a flame-spread index of 5 and a smoke density index of 15, according to the manufacturer.

Just Like New Overspray Management
Modern Safety Techniques

PyroTech, based in Addison, IL, formulates, manufactures, and tests flame retardant chemical coatings around the globe.

Tarps manufacturing, Inc.
base painters

More information: www.pyrotech.us.

Tagged categories: Coating Materials; Coatings Technology; Fire; Intumescent; Wood; Wood coatings