A researcher at Johns Hopkins University set out to develop an environmentally friendly coating to deflect the damaging heat and rays of the sun and prolong the life of metal structures.
What he came up with was an innovative coating made out of glass that can be used on metal surfaces in applications ranging from naval ships to rooftops.
Inspired by Glass
Jason J. Benkoski, Ph.D., senior scientist in the Johns Hopkins University Applied Physics Lab, chose to work with glass, which is made out of silica, for his ideal coating because it is hard, durable and has the right optical properties.
American Chemical Society |
Benkoski's silica-based coating, for use on military ships and other metal surfaces, can expand and contract with fluctuating air temperatures, reflect sunlight and resist water. |
He told Forbes magazine, his lab was inspired by the durability of paints known as “water glass.” “The starting materials are the cheapest things you can imagine—sand and potash,” he said.
The long-standing facades in Germany and Switzerland were given as an example of the exterior use of water glass paints—they likely have maintained their splendor over time because the glass reflected sunlight.
Water glass paints required a clean rough surface to cling to, though, which doesn’t make them a good match for metal, Benkoski explained.
At Work in the Lab
In the lab, Benkoski began with silica, one of the most abundant materials in the Earth’s crust, and modified one version of it, potassium silicate, that normally dissolves in water. His tweaks transformed the compound so that when it’s sprayed onto a surface and dries, it becomes water resistant.
Benkoski explained the logic behind his research: “Most paints you use on your car or house are based on polymers, which degrade in the ultraviolet light rays of the sun. So over time you’ll have chalking and yellowing.
“Polymers also tend to give off volatile organic compounds, which can harm the environment. That’s why I wanted to move away from traditional polymer coatings to inorganic glass ones,” he said in a release from the American Chemical Society.
American Chemical Society |
This silica-based coating is designed to keep an outdoor metal surface close to air temperature and thereby slow down corrosion and other types of degradation. |
Unlike acrylic, polyurethane or epoxy paints, Benkoski’s paint is almost completely inorganic, which should make it last far longer than its counterparts that contain organic compounds, according to the ACS. His paint is also designed to expand and contract with metal surfaces to prevent cracking.
Mixing pigments with the silicate gives the coating an additional property: the ability to reflect all sunlight and passively radiate heat. Since it doesn’t absorb sunlight, any surface coated with the paint will remain at air temperature, or even slightly cooler. That’s key to protecting structures from the sun.
“When you raise the temperature of any material, any device, it almost always by definition ages much more quickly than it normally would,” Benkoski said.
“It’s not uncommon for aluminum in direct sunlight to heat 70 degrees Fahrenheit above ambient temperature. If you make a paint that can keep an outdoor surface close to air temperature, then you can slow down corrosion and other types of degradation.”
“It’s almost like painting a rock on top of your metal. And this is going to last not tens of years but maybe hundreds of years,” he said in National Geographic.
Applications in the Field
The paint Benkoski’s lab is developing is intended for use on naval ships (some funding for his work was provided by the U.S. Office of Naval Research), but it has other potential commercial applications, including as a cool roof coating.
“You might want to paint something like this on your roof to keep heat out and lower your air conditioning bill in the summer,” he said.
“White paint by itself does a good job,” reflecting about 90 percent of the sun’s energy, he told National Geographic.
But, he explained, a polymer-based coating cannot reject ultraviolet light like a silica-based paint can. “With as little as three years of UV degradation, a polymer paint could absorb twice as much solar energy as it did when freshly painted,” he added.
Mixing pigments with the silicate gives the coating the ability to reflect sunlight and passively radiate heat. |
He suggested the paint could also go on metal playground slides or bleachers. And it would be affordable. The materials needed to make the coating are abundant and inexpensive.
He indicated he also expects to find applications for ceramics such as glass, concrete and rock, as well as fiberglass or previously polymer-painted surfaces.
Development Schedule
Not yet on the market, Benkoski says he expects his lab will start field testing the material in about two years.
He told National Geographic it could take five years for the product to reach the commercial market, and he expects the paint’s chances for success will be bolstered by the Navy’s sponsorship of his research.