Coating manufacturer Jotun (Sandefjord, Norway) recently introduced a new high-temperature coating designed for use in the hydrocarbon processing industry.

Hydrocarbon processing
Jotun
Jotatemp 1000 Ceramic is designed for the temperature demands of the hydrocarbon processing industry.
Hydrocarbon processing
Jotun

Jotatemp 1000 Ceramic is designed for the temperature demands of the hydrocarbon processing industry.

Jotatemp 1000 Ceramic is a corrosion-protection coating that the company says can be applied to surfaces that reach up to 1,000 degrees Celsius (1,832 degrees Fahrenheit).

Industry Demand

The company says the product comes in response to demand from the industry.

“The on-shore industry is moving towards higher temperature processing, while still requiring low temperature tolerance for gas processing, and needs a coating with performance credentials to match its ambitions,” said Miles Bruckhurst, Jotun global concept director, hydrocarbon processing industry.

Modern Safety Techniques
Tarps manufacturing, Inc.

The coating provides protection from corrosion, fire, heat and cold, Jotun says, and passed all industry standard tests for the verification of corrosion-under-insulation protection.

Coating Details

NLB Corporation
Just Like New Overspray Management

Jotatemp 1000 Ceramic is a two-component titanium-catalyzed inorganic ceramic copolymer, according to Jotun. The company recommends application via airless spray, with brush application for stripe coating and small areas.

Jotun recommends the coating for properly prepared carbon steel, stainless steel and ceramic surfaces.

Quikspray, Inc.
base painters

More information: www.jotun.com.

Tagged categories: Carbon Steel; Ceramic coatings; Coating Materials; Industrial coatings; Jotun; Oil and Gas; Stainless steel