G85 Standard Practice for Modified Salt Spray (Fog) Testing

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 08, 2011
Updated On: August 29, 2011
Editorial Change:
 
This practice is applicable to ferrous and nonferrous metals; also organic and inorganic coatings. The variations described herein are useful when a different or more corrosive environment than the salt fog described in Practice B 117 is desired.

1.1 This practice covers and sets forth conditions for five modifications in salt spray (fog) testing for specification purposes. These are in chronological order of their development: 1.1.1 Annex A1, acetic acid-salt spray test, continuous. 1.1.2 Annex A2, cyclic acidified salt spray test. 1.1.3 Annex A3, seawater acidified test, cyclic (SWAAT). 1.1.4 Annex A4, SO2 salt spray test, cyclic. 1.1.5 Annex A5, dilute electrolyte cyclic fog dry test.

1.2 This practice does not prescribe the type of modification, test specimen or exposure periods to be used for a specific product, nor the interpretation to be given to the results.

(Back to all Standards)

 
   

Atlantic Design, Inc.
Rentals, Rentals & More

Our rental fleet has grown and
now includes newer models
with our enhanced safety
features and recent
upgrades. Call today for rates. 866.Call.ADI


Abrasives Inc.
Check our Prices for Blast Abrasives

Faced with higher abrasive costs? We invite you to call & check our rates on Black Magic® coal slag and other quality blast materials. Abrasives Inc. 800-584-7524


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Pipeline Utility Aerial crossings coated since 1992. Termarust's (HR CSA) was used to overcoat lead paint and preserve cables, pipes and support towers.


Madison Chemical Industries Inc.
Coat steel without blasting

Madison’s No-Blast technology
eliminates the need for
abrasive blasting in a number
of service applications.
See it in action at
MadisonChemical.com.


Axxiom Manufacturing
Schmidt Introduces
the New miniBRS

Reduced in size, it is incredibly easy to maneuver and operate! The perfect alternative to larger blast & recovery units when project space is limited.
Call 1-800-231-2085


MMLJ
Superfast Dustless Abrasive Blasting - Watch Video

Dustless Blasting creates no dust plume so others can work nearby unaffected. Maximize Productivity! Watch our numerous YouTube videos to learn more.


SAFE Systems, Inc.
Portable Dust Collectors for Tough Environments

Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com