D3170 Standard Test Method for Chipping Resistance of Coatings

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: October 08, 2012
Updated On: October 09, 2012
Editorial Change:
 
Owners consider chipping of coatings, particularly on the leading faces and edges of automobile surfaces, unacceptable. In formulating a coating or coating system to meet service requirements, the resistance to chipping damage by flying objects such as gravel is one of the properties of importance since it can vary considerably as other properties are adjusted. Since resistance to chipping decreases at lower temperatures partly as the result of decreased flexibility, the test may be more directly related to service conditions by performing it at a low temperature. This test method is designed to produce a controlled amount of impact by the media on the coated panel in order to enhance reproducibility.

(Back to all Standards)

 
   

ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


Safety Lamp of Houston, Inc.
Wet & hazardous area lighting solutions from SAFETY LAMP of Houston

New WOLF LED and fluorescent lights are now available, including low voltage tank lighting kits.
Call: (281) 964-1019.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


Atlantic Design, Inc.
We’ve Got a Surprise For You!

We’ve designed two new lines
of equipment with shorter lead
times, budget friendly prices,
more safety features & all
with the same ADI quality!
866.Call.ADI


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


International Bridge Conference
International Bridge Conference

Join us in Pittsburgh over June 2-6, 2013 to celebrate the 30th Anniversary of the International Bridge Conference®, the world’s premier technical conference on bridges.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated with Termarust's (HR CSA) in 1995. This highway & rail truss bridge is still stable and there still is no active corrosion.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com