G15 Standard Terminology Relating to Corrosion and Corrosion Testing

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: May 29, 2008
Editorial Change:
 
1.1 This terminology covers commonly used terms in the field of corrosion. Related terms may be found in Terminologies D 16, D 4538, G 40, or other ASTM terminology standards. All terms defined by ASTM committees may be found in the ASTM Dictionary of Engineering Technology.

(Back to all Standards)

 
   

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


MMLJ
Superfast Dustless Abrasive Blasting - Watch Video

Dustless Blasting creates no dust plume so others can work nearby unaffected. Maximize Productivity! Watch our numerous YouTube videos to learn more.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


EDCO - Equipment Development Co. Inc.
EDCO's Quick Response Codes

EDCO now includes Quick Response Code decals on machines. These QRC's provide customers with instant jobsite advice, problem solving tips and much more. Click to watch EDCO machines in action.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com