How Coatings Perform over Waterjetting in New Construction

From JPCL, September 2011

More items for Surface Preparation

by Philippe Le Calvé, DCNS, France; Jean-Pierre Pautasso, Direction Générale pour I’Armement, France; and Nathalie le Bozec, French Corrosion Institute, France

The authors report on the performance of commonly used paint systems for the protection of ship exterior topsides applied on zinc shop-primed steel after abrasive cleaning and after UHP waterjetting. The article compares the condition of several paint systems after a series of tests....
(Login to read the full article)

   

Tagged categories: Shop-applied coatings; Steel; UHP waterjetting; Waterjetting

Comment Join the Conversation:

Sign in to our community to add your comments.

Axxiom Manufacturing
Schmidt Improves Conversion Kits

Schmidt's conversion kits turn out-of-date blast pots into high quality, efficient blasters. Quick, easy to install with step by step instructions.
Call 1-800-231-2085


CHLOR*RID International Inc.
Surface cleanliness is
ESSENTIAL to coating
performance.

* TEST FOR SALTS
* PREVENT FLASH RUST
* REMOVE SALTS
More information at
www.chlor-rid.com,

800-422-3217


Atlantic Design, Inc.
We’re Ahead of the Game Now!

ADI has been in production all winter and our newest equipment lines are now in stock and ready to go. Buy, rent, or trade, but they will be going fast! 866.Call.ADI


Harsco
BLACK BEAUTY® GLASS

A 100% post-consumer bottle glass abrasive from a company you can trust. Toll Free: 1-888-733-3646


Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.


ITW Polyspec
FLEX IMO
for Marine Deck Coating

FLEX IMO is a uniquely formulated decorative polymer deck coating system that combines aesthetics and fire safety. FLEX IMO is an IMO approved coating system.


Novatek Corporation
Dustless Coatings Removal

Strip it, clean it, and profile it,
all dust free! High production
rates and Blast like finishes.
Comply with new lead
standards.

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com